Investigation of the Near Surface Mechanical Properties of Ammonium Perchlorate by Nanoindentation
(Oklahoma State University, 2004-05-01)
The mechanical response of crystalline energetic solids to force loading is known to play a role in thermal decomposition, and also contributes to the overall mechanical behavior of the composite solid propellant. Ammonium ...