Investigation of the Near Surface Mechanical Properties of Au-ti Thin Films
(Oklahoma State University, 2008-07-01)
Gold is a common metal chosen for MEMS electrical contacts because of its high conductivity, ductility, inertness, and low resistivity, contact resistance and susceptibility to oxidation. However, due to the low hardness ...