Effects of ion irradiation on the microstructure and mechanical properties of titanium-based metallic glasses
(2019-08)Metallic glass specimens with a nominal composition of Ti₄₀Cu₃₄-ₓPd₁₄Zr₁₀Sn2Siₓ (at.%), where x = 2, 3, and 5, were subjected to annealing and/or ion irradiation and their microstructure and mechanical properties were ... -
Exploratory Investigation of Viscoelastic Nanoindentation on Polyvinyl Acetate
(Oklahoma State University, 2009-05-01)Nanoindentation load-displacement data of polyvinyl acetate (PVAc) was obtained at different temperatures ranging from ~20 oC to 42 oC using two novel equipments, Hysitron Triboindenter and Interfacial Force Microscopy ... -
Investigation of the Near Surface Mechanical Properties of Ammonium Perchlorate by Nanoindentation
(Oklahoma State University, 2004-05-01)The mechanical response of crystalline energetic solids to force loading is known to play a role in thermal decomposition, and also contributes to the overall mechanical behavior of the composite solid propellant. Ammonium ... -
Investigation of the Near Surface Mechanical Properties of Au-ti Thin Films
(Oklahoma State University, 2008-07-01)Gold is a common metal chosen for MEMS electrical contacts because of its high conductivity, ductility, inertness, and low resistivity, contact resistance and susceptibility to oxidation. However, due to the low hardness ... -
Multiscale modeling and simulation: Incorporation of mesoplasticity between atomistic and continuum
(2007-08)Scope and Method of Study: In the framework of multiscale modeling, two modeling techniques at the meso/micro scale, namely, mesoplasticity and discrete dislocation are employed to study the mechanical behavior of single ... -
Residual stress in all ceramic zirconia-porcelain dental system by simulation and nanoindentation
(2012-07)Scope and Method of Study: